{"_buckets": {"deposit": "a09731cb-b6af-4e0c-b059-034306d21a01"}, "_deposit": {"created_by": 1, "id": "22202", "owners": [1], "pid": {"revision_id": 0, "type": "depid", "value": "22202"}, "status": "published"}, "_oai": {"id": "oai:u-fukui.repo.nii.ac.jp:00022202", "sets": ["2404"]}, "author_link": ["63823", "63824", "63828", "63827", "63826", "63825"], "item_10001_biblio_info_7": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "2006-07", "bibliographicIssueDateType": "Issued"}, "bibliographicIssueNumber": "1", "bibliographicPageEnd": "118", "bibliographicPageStart": "112", "bibliographicVolumeNumber": "261", "bibliographic_titles": [{"bibliographic_title": "Wear"}]}]}, "item_10001_description_5": {"attribute_name": "抄録", "attribute_value_mlt": [{"subitem_description": "In this paper, it is proposed to use a new type of solid particle impact test (slurry jet) to swiftly evaluate wear properties of thin, single layered or multilayered coatings. By the slurry jet, 1.2 µm alumina particles were impacted at high velocity perpendicular to thin PVD coatings of TiN deposited on high speed steel substrate materials under various substrate temperatures. Since the coatings have a much higher wear resistance than the substrate material, the wear rate increases significantly to the higher level of the HSS material when the coatings are penetrated. This is utilized in the quantification of the assessment of coating wear. A ranking of wear resistance and correlations to the coating surface hardness measured by nano-indentation tests, and coating morphology and structures are given and discussed. It is concluded that the slurry jet test is fast, easy to accomplish, and generates reproducible results. It is also very sensitive to variations in coating quality. Thus, it can be recommended as a screening test when evaluating coatings and coated materials. For the coatings included in this study, the TiN deposited under the highest substrate temperature proved to have the highest wear resistance although it had a relatively low hardness. The wear rate of the TiN coatings varies with the orientation of grains, that is, the {111} orientation that dominates for the high temperature deposition shows a higher wear resistance than the {100} orientation, which corresponds with the cleavage fracture behavior. The fact that the higher temperature generates more defect free TiN coatings will also contribute to a better erosive wear resistance for these coatings.", "subitem_description_type": "Abstract"}]}, "item_10001_publisher_8": {"attribute_name": "出版者", "attribute_value_mlt": [{"subitem_publisher": "Elsevier Ltd"}]}, "item_10001_relation_11": {"attribute_name": "書誌レコードID", "attribute_value_mlt": [{"subitem_relation_type_id": {"subitem_relation_type_id_text": "TD00006649", "subitem_relation_type_select": "NCID"}}]}, "item_10001_relation_14": {"attribute_name": "DOI", "attribute_value_mlt": [{"subitem_relation_type": "isVersionOf", "subitem_relation_type_id": {"subitem_relation_type_id_text": "10.1016/j.wear.2005.09.030", "subitem_relation_type_select": "DOI"}}]}, "item_10001_source_id_9": {"attribute_name": "ISSN", "attribute_value_mlt": [{"subitem_source_identifier": "431648", "subitem_source_identifier_type": "ISSN"}]}, "item_10001_version_type_20": {"attribute_name": "著者版フラグ", "attribute_value_mlt": [{"subitem_version_resource": "http://purl.org/coar/version/c_b1a7d7d4d402bcce", "subitem_version_type": "AO"}]}, "item_creator": {"attribute_name": "著者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "IWAI, Y"}], "nameIdentifiers": [{"nameIdentifier": "63823", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "MIYAJIMA, T"}], "nameIdentifiers": [{"nameIdentifier": "63824", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "HONDA, T"}], "nameIdentifiers": [{"nameIdentifier": "63825", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "MATSUBARA, T"}], "nameIdentifiers": [{"nameIdentifier": "63826", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "KANDA, K"}], "nameIdentifiers": [{"nameIdentifier": "63827", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "HOGMARK, S"}], "nameIdentifiers": [{"nameIdentifier": "63828", "nameIdentifierScheme": "WEKO"}]}]}, "item_files": {"attribute_name": "ファイル情報", "attribute_type": "file", "attribute_value_mlt": [{"accessrole": "open_date", "date": [{"dateType": "Available", "dateValue": "2020-08-04"}], "displaytype": "detail", "download_preview_message": "", "file_order": 0, "filename": "BD00006649_001.pdf", "filesize": [{"value": "1.0 MB"}], "format": "application/pdf", "future_date_message": "", "is_thumbnail": false, "licensetype": "license_free", "mimetype": "application/pdf", "size": 1000000.0, "url": {"label": "BD00006649_001.pdf", "url": "https://u-fukui.repo.nii.ac.jp/record/22202/files/BD00006649_001.pdf"}, "version_id": "a46ce1c1-9307-488e-af82-abc13ad97da1"}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "eng"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "other", "resourceuri": "http://purl.org/coar/resource_type/c_1843"}]}, "item_title": "EVALUATION OF EROSIVE WEAR RESISTANCE OF TiN COATINGS BY A SLURRY JET IMPACT TEST", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "EVALUATION OF EROSIVE WEAR RESISTANCE OF TiN COATINGS BY A SLURRY JET IMPACT TEST"}]}, "item_type_id": "10001", "owner": "1", "path": ["2404"], "permalink_uri": "http://hdl.handle.net/10098/1163", "pubdate": {"attribute_name": "公開日", "attribute_value": "2007-11-14"}, "publish_date": "2007-11-14", "publish_status": "0", "recid": "22202", "relation": {}, "relation_version_is_last": true, "title": ["EVALUATION OF EROSIVE WEAR RESISTANCE OF TiN COATINGS BY A SLURRY JET IMPACT TEST"], "weko_shared_id": -1}
EVALUATION OF EROSIVE WEAR RESISTANCE OF TiN COATINGS BY A SLURRY JET IMPACT TEST
http://hdl.handle.net/10098/1163
http://hdl.handle.net/10098/1163b7620587-448a-4bbe-a759-d1838f825325
名前 / ファイル | ライセンス | アクション |
---|---|---|
BD00006649_001.pdf (1.0 MB)
|
|
Item type | 学術雑誌論文 / Journal Article(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2007-11-14 | |||||
タイトル | ||||||
タイトル | EVALUATION OF EROSIVE WEAR RESISTANCE OF TiN COATINGS BY A SLURRY JET IMPACT TEST | |||||
言語 | ||||||
言語 | eng | |||||
資源タイプ | ||||||
資源タイプ識別子 | http://purl.org/coar/resource_type/c_1843 | |||||
資源タイプ | other | |||||
著者 |
IWAI, Y
× IWAI, Y× MIYAJIMA, T× HONDA, T× MATSUBARA, T× KANDA, K× HOGMARK, S |
|||||
抄録 | ||||||
内容記述タイプ | Abstract | |||||
内容記述 | In this paper, it is proposed to use a new type of solid particle impact test (slurry jet) to swiftly evaluate wear properties of thin, single layered or multilayered coatings. By the slurry jet, 1.2 µm alumina particles were impacted at high velocity perpendicular to thin PVD coatings of TiN deposited on high speed steel substrate materials under various substrate temperatures. Since the coatings have a much higher wear resistance than the substrate material, the wear rate increases significantly to the higher level of the HSS material when the coatings are penetrated. This is utilized in the quantification of the assessment of coating wear. A ranking of wear resistance and correlations to the coating surface hardness measured by nano-indentation tests, and coating morphology and structures are given and discussed. It is concluded that the slurry jet test is fast, easy to accomplish, and generates reproducible results. It is also very sensitive to variations in coating quality. Thus, it can be recommended as a screening test when evaluating coatings and coated materials. For the coatings included in this study, the TiN deposited under the highest substrate temperature proved to have the highest wear resistance although it had a relatively low hardness. The wear rate of the TiN coatings varies with the orientation of grains, that is, the {111} orientation that dominates for the high temperature deposition shows a higher wear resistance than the {100} orientation, which corresponds with the cleavage fracture behavior. The fact that the higher temperature generates more defect free TiN coatings will also contribute to a better erosive wear resistance for these coatings. | |||||
書誌情報 |
Wear 巻 261, 号 1, p. 112-118, 発行日 2006-07 |
|||||
出版者 | ||||||
出版者 | Elsevier Ltd | |||||
ISSN | ||||||
収録物識別子タイプ | ISSN | |||||
収録物識別子 | 431648 | |||||
書誌レコードID | ||||||
識別子タイプ | NCID | |||||
関連識別子 | TD00006649 | |||||
DOI | ||||||
関連タイプ | isVersionOf | |||||
識別子タイプ | DOI | |||||
関連識別子 | 10.1016/j.wear.2005.09.030 | |||||
著者版フラグ | ||||||
出版タイプ | AO | |||||
出版タイプResource | http://purl.org/coar/version/c_b1a7d7d4d402bcce |