Počet záznamů: 1  

Possibilites of using the Erichsen test for determination of forming limit diagram and its utilization for hydroforming

  1. 1.
    0485657 - ÚPT 2018 RIV CZ eng C - Konferenční příspěvek (zahraniční konf.)
    Řiháček, J. - Mrňa, Libor - Peterková, E. - Dvořák, M.
    Possibilites of using the Erichsen test for determination of forming limit diagram and its utilization for hydroforming.
    METAL 2017. 26th International Conference on Metallurgy and Materials. Conference Proceedings. Ostrava: TANGER, 2017, s. 286-391. ISBN 978-80-87294-79-6.
    [METAL 2017: International Conference on Metallurgy and Materials /26./. Brno (CZ), 24.05.2017-26.05.2017]
    Institucionální podpora: RVO:68081731
    Klíčová slova: Erichsen test * formability * hydroforming * FLD
    Obor OECD: Optics (including laser optics and quantum optics)

    Forming limit diagrams (FLD) are used to determine process limitations in sheet metal forming, i.e. as a level of formability assisting in the estimation of stamping characteristics. This paper deals with the experimental determination of a forming limit curve (FLC) using the Erichsen test. In this case, FLC of an austenitic stainless
    steel X5CrNi18-10 is obtained by performing the Erichsen test with different shapes of specimens. Furthermore, utilization of FLD for evaluation of a hydroforming process is shown in the second part of the paper.