タイトル: Activities of FeO and P₂O₅ in dephosphorization slags Co existing with solid solutions between di-calcium silicate and tri-calcium phosphate
著者: Matsugi, Ryota
Miwa, Kohei
Hasegawa, Masakatsu  kyouindb  KAKEN_id
著者名の別形: 松儀, 亮太
三輪, 紘平
長谷川, 将克
キーワード: dephosphorization
activity
di-calcium silicate
tri-calcium phosphate
solid solution
発行日: Oct-2017
出版者: Iron and Steel Institute of Japan
誌名: ISIJ International
巻: 57
号: 10
開始ページ: 1718
終了ページ: 1724
抄録: Towards better understanding of the phosphorus removal from hot metal with low-basicity slags, electrochemical technique incorporating MgO-stabilized zirconia was conducted to measure simultaneously the activities of FeO and P₂O₅ within heterogeneous CaO–SiO₂–P₂O₅–FeO slags. The FeO activity was fairly insensitive to the variation of Ca₃P₂O₈ content in solid solutions between Ca₂SiO₄–Ca₃P₂O₈, while the P₂O₅ activity increased with an increase in Ca₃P₂O₈ content. By using the present values for activities, phosphorus distribution ratios were estimated between molten slag and carbon-saturated iron. The relationship between phosphorus distribution ratio and FeO content in molten slag was consistent with the phase diagram of the pseudo-ternary CaO–(SiO₂–P₂O₅)–FeO system.
著作権等: © 2017 The Iron and Steel Institute of Japan.
This is an open access article under the terms of the Creative Commons Attribution-NonCommercial-NoDerivs license.
URI: http://hdl.handle.net/2433/265373
DOI(出版社版): 10.2355/isijinternational.ISIJINT-2017-082
出現コレクション:学術雑誌掲載論文等

アイテムの詳細レコードを表示する

Export to RefWorks


出力フォーマット 


このアイテムは次のライセンスが設定されています: クリエイティブ・コモンズ・ライセンス Creative Commons